IMPACT COUPLER · Coupler tulangan dengan baut
Satu kali kencangkan,
sambungan tulangan tanpa slip.
IMPACT COUPLER is structural technology, not just a material. No flame, no end threading, no special equipment: tighten the bolt with a standard impact tool and axial tension pre-compresses the rebar, blocking initial slip.
Mengapa sambungan baru
Apakah sambungan tulangan di proyek Anda sudah cukup baik?
Risiko kebakaran & ledakan
Gas pressure welding carries fire, explosion and heat-affected-zone weakening risks. Under Korea's Serious Accidents Punishment Act, flame-free methods are urgent.
Kekurangan tenaga ahli
Workers in their 20s and 30s fell from 56.6% of Korea's construction workforce in 1995 to 21.6% in 2024, with a shortfall estimated at about 350,000 people.
Standar tahan gempa lebih ketat
KCI-ST103:2026 tightens dynamic performance evaluation of splices. Existing couplers with inconsistent fastening struggle to comply.
Pemborosan sambungan lewatan
Lap splices overlapping 600 mm or more waste about 15% of rebar — over KRW 120 billion a year — and congested bars cause poor concrete filling.
Cara kerja
Mengubah putaran menjadi tarikan.
Struktur pra-tekan (Pre-tensioning).
Rotational impact energy from the wrench becomes axial tension that physically pre-compresses the rebar. Multi-point bolt pressure and a radial expansion mechanism lock the rebar ribs and grippers together with zero play, blocking the slip that occurs when load is first applied.
3 related patent applications (Feb 2026) · axial tension pressing · radial expansion mechanism
-
STEP 1
Pasang tulangan bawah
Tanpa pengguliran ulir — pasang tulangan apa adanya.
-
STEP 2
Pasang tulangan atas
Masukkan tulangan dari sisi seberang. Bisa untuk tulangan vertikal, horizontal, dan sengkang.
-
STEP 3
Kencangkan baut (selesai)
5–10 detik dengan alat impact standar sekitar 3 kg. Torsi acuan (N·m) langsung memastikan pemasangan selesai.


Perbandingan
Komponen lebih sedikit, lebih kuat, lebih cepat.
| Item | Sambungan lewatan | Tipe ulir | Las tekan gas | Tipe baji | IMPACT COUPLER |
|---|---|---|---|---|---|
| Material | - | S45C | - | S45C | SCM440 |
| Mutu tulangan | SD400 | SD500 | SD400 | SD500 | SD600 |
| Kuat tarik | - | 570~700 MPa | - | 570~700 MPa | 850~1,000 MPa (target) |
| Waktu pemasangan | 2 hari lebih | 10–30 menit | 10–20 menit | 5–10 menit | Kurang dari 1 menit |
| Risiko kebakaran | Tidak ada | Tidak ada | Sangat tinggi | Tidak ada | Tidak ada |
| Ketergantungan keahlian | Tinggi | Tinggi | Sangat tinggi | Sedang | Tidak perlu |
| Kontrol mutu | Visual | Torsi manual | Manual | Manual | Pemetaan torsi digital |
Time per splice is from the product catalog; the table is based on the 2026 business plan. IMPACT COUPLER tensile strength is a development target with SCM440.
Spesifikasi
Siap untuk tulangan mutu sangat tinggi SD600 dengan baja paduan SCM440.
Plain carbon steel (S45C) struggles to stay uniformly strong through large diameters. We quench (830–870 °C, oil) and temper (500–650 °C) Cr-Mo alloy steel SCM440 for both strength and toughness.

- Metode
- High-strength axial tension bolt fastening (pre-tensioning)
- Tulangan
- SD400~SD600 · D13~D43 (10 ukuran)D22 and D25 prototypes first; other sizes to follow
- Material
- SCM440 alloy steel, Q/T heat-treated · HRC 32+
- Kuat tarik
- Prototype measured at 611 N/mm²Target 850–1,000 MPa with SCM440
- Pemasangan & gempa
- Under 1 min · targeting KCI-ST103 seismic grade 1Residual slip ≤ 0.1 mm, 30+ load cycles
- Permesinan
- NC/CNC precision machining, ±0.05 mm tolerance
Tabel ukuran
10 ukuran dari D13 hingga D43
| Ukuran tulangan | D13 | D16 | D19 | D22 | D25 | D29 | D32 | D35 | D38 | D43 |
|---|---|---|---|---|---|---|---|---|---|---|
| Diameter luar D (mm) | 35 | 40 | 48 | 55 | 60 | 68 | 70 | 75 | 80 | 86 |
| Panjang L (mm) | 92 | 105 | 130 | 146 | 163 | 182 | 197 | 205 | 212 | 220 |
Dimensions from the product catalog; they may change in mass production.
Kinerja & sertifikasi
Kami memisahkan apa yang sudah terbukti dan apa yang masih diuji.
Terbukti Hasil sejauh ini
- Tensile test: 611 N/mm² measuredGyeongsang National University, Dept. of Civil Engineering · above the KS B 0802 reference of 560 N/mm²
- 3 patent applications (Feb 2026)Impact-fastened axial tension pressing · impact screw-fastened radial expansion · radial expansion mechanism and installation method
Berjalan Peta jalan sertifikasi
- KS B 0802 accredited test reportTensile strength report from an accredited laboratory
- KCI-ST103:2026 seismic grade 1Residual slip ≤ 0.1 mm, 30+ cyclic loads
- ISO 15835 · Korean New Construction TechnologyCertifications for export and public procurement


Laporan Uji →
Download published test reports as PDF.
Aplikasi
Dari apartemen hingga pembangkit listrik — di mana pun sambungan penting.
Apartemen & gedung komersial
Fast, uniform splicing for mat foundations and columns
Fondasi turbin & menara pendingin
Structures under constant vibration, dynamic load and fatigue
Tangki penyimpanan LNG
Special structures for cryogenic and airtight conditions
Jembatan, pelabuhan & terowongan
Infrastructure and coastal structures with mandatory seismic design
KORINGO Co., Ltd.
Rebar splicing technology for safer, more efficient sites.
IMPACT COUPLER is KORINGO's construction technology business. KORINGO also runs a native-language Korean learning platform and a platform development business.
Minta Penawaran
Tell us about your site and we will send a quote with the right sizes.
- Telepon
- +82 55-759-1026
- kimgk1026@gmail.com
Minta penawaran hanya satu menit
Leave the rebar size, estimated quantity and site location, and we will contact you within 1–2 business days. Drawings or quantity sheets help us be precise.
Minta penawaran